We are glad to introduce our company as a Hi-Tech alloying solution of different elements for de-sulpharisation, de-oxidization into molten steel treatment by Wire injection technology to produce quality steel.
POWDER SPECIFICATION FOR CaSi:
Ca-28-30%, Si-55-65%, Al-1.5%max, C-1%max, S-0,03%max
P-0,03%max and Fe-4-8%
Wire Dia: 13 mm+/- 0.25 mm
Shape: Round
Sheath: + 0.04 mm
Powder Fill Rate (avg): 200 +/- 10 gm per meter
Type of Coil: Flipping
Axis : Horizontal / Vertical
Powder Weight/Coil: 1000 - 1200 Kg
We'll be glad to receive your detailed inquiries.
Thanks for your kind attention and best regards. If you require